Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -120 °C | -184 °F | |
Precision Polymer Engineering S65E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 65-75 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. Meets UK Ministry of Defence aerospace specifica.. |
|||
Minimum Service Temperature, Air | -120 °C | -184 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering S65E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 65-75 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. Meets UK Ministry of Defence aerospace specifica.. |
|||
Minimum Service Temperature, Air | -120 °C | -184 °F | DSC |
Adamas Adalon® 209 PTFE, 15% Glass Filled Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -120 °C | -184 °F | DSC |
Adamas Adalon® 215 PTFE, 17% Glass Filled, Blue Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -120 °C | -184 °F | DSC |
Adamas Adalon® 902 PTFE, 1% Conductive filler Information provided by Adamas, HPM |