Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.38 MPa | 1360 psi | ASTM D412 |
Polymax® Maxelast® P3877 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 9.38 MPa | 1360 psi | ASTM D412 |
Polymax® Maxelast® P3880 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 9.38 MPa | 1360 psi | ASTM D412 |
Precision Polymer Engineering C70R Chloroprene Rubber Red Iron Oxide filled, Chloroprene Rubber, 66-75 °IRHD. Flame retarding.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils. .. |
|||
Tensile Strength, Yield | 9.35 MPa | 1360 psi | -15% change after 168 hours @ 125°C; ASTM D412 |
Precision Polymer Engineering E70E Ethylene Propylene Rubber Ethylene Propylene Terpolymer, 66-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet Aerospace Specification DTD5597A Grade 70.Applications: For sealing applications where goo.. |
|||
Tensile Strength, Yield | 9.40 MPa | 1360 psi | ASTM D412 |
Precision Polymer Engineering S65E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 65-75 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. Meets UK Ministry of Defence aerospace specifica.. |
|||
Tensile Strength, Yield | 9.35 MPa | 1360 psi | 10% change after 168 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S80U Silicone Rubber Translucent Silicone Rubber, 70 -80 °IRHD. Shore A Platinum cured Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Silicone compound in conformity with the req.. |
|||
Tensile Strength, Yield | 9.40 MPa | 1360 psi | ASTM D638 |
NOVA Chemicals Novapol® LM-2522-A LDPE Injection Molding Resin Features: Medium flow LDPE with a good balance of toughness, softness, dimensional stability and processability Applications: Injection molding of caps, closures and other specialty productsInformat.. |
|||
Tensile Strength, Yield | 9.40 MPa | 1360 psi | ASTM D638 |
NOVA Chemicals Novapol® LM-4021-L LDPE Injection Molding Resin Features: Medium flow LDPE with a good balance of toughness, softness, dimensional stability and processability Applications: Injection molding of caps, closures and other specialty productsInformat.. |
|||
Tensile Strength, Yield | 9.40 MPa @Strain 300 % |
1360 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1685AE Polyether TPU Resin ISOTHANE 1600 series products are polyether based thermoplastic polyurethanes with good balanced qualities. They exhibit high moisture vapor transmission. The product can be e xtruded and blowed.Inf.. |
|||
Tensile Strength, Yield | >= 9.38 MPa | >= 1360 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7344 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 9.40 MPa @Strain 300 % |
1360 psi @Strain 300 % |
ASTM D412 |
Dow SE SLR-4610 H Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-4610 H is manufactured by anionic solution polymerization using lithium initiator and is extended with 37.5 parts of aromatic oil in relation to solid rubber. It is a product with medium sty.. |