Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -184 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -120 °C
-184 °F
Precision Polymer Engineering S65E Silicone Rubber
Red iron oxide filled, Phenyl Silicone Rubber, 65-75 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. Meets UK Ministry of Defence aerospace specifica..
Minimum Service Temperature, Air -120 °C
-184 °F
Non-brittle after 3 minutes
Precision Polymer Engineering S65E Silicone Rubber
Red iron oxide filled, Phenyl Silicone Rubber, 65-75 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. Meets UK Ministry of Defence aerospace specifica..
Minimum Service Temperature, Air -120 °C
-184 °F
DSC
Adamas Adalon® 209 PTFE, 15% Glass Filled
Information provided by Adamas, HPM
Minimum Service Temperature, Air -120 °C
-184 °F
DSC
Adamas Adalon® 215 PTFE, 17% Glass Filled, Blue
Information provided by Adamas, HPM
Minimum Service Temperature, Air -120 °C
-184 °F
DSC
Adamas Adalon® 902 PTFE, 1% Conductive filler
Information provided by Adamas, HPM
Copyright © lookpolymers.com All Rights Reserved