Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamTal PMH2010 Polyacetal Homopolymer for Injection Molding

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamTal PMH2010 Polyacetal Homopolymer for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose polyacetal homopolymer for injection molding applications, MFI 10.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ISO 2577
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ISO 527
Elongation at Break 60 %
60 %
ISO 527
Flexural Strength 105 MPa
15200 psi
ISO 178
Flexural Modulus 3.00 GPa
435 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Users viewing this material also viewed the following: