Polyram RamLloy PN300G6 PPE/PS Alloy, 30% Glass Fiber

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene + Polyphenylene Ether, Glass Filler
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamLloy PN300G6 PPE/PS Alloy, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE/PS alloy, 30% glass fiber reinforced for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.0060 %
0.0060 %
50% RH; ISO 62
Water Absorption at Saturation 0.20 %
0.20 %
ISO 62
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ISO 2577
Melt Flow 5.0 g/10 min

@Load 10.0 kg,
Temperature 280 °C
5.0 g/10 min

@Load 22.0 lb,
Temperature 536 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 7.90 GPa
1150 ksi
ISO 527
Flexural Strength 130 MPa
18900 psi
ISO 178
Flexural Modulus 7.30 GPa
1060 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Dielectric Strength 18.0 kV/mm
457 kV/in
IEC 60250