Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastics Duracon® CH-20 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Carbon Fiber Filled
Manufacturer Polyplastics Co.
Trade Name Duracon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastics Duracon® CH-20 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O) and carbon-carbon (-C-C- bond) comonomer groups are incorporated into its main chain. Therefore the copolymer has superior chemical and thermal stability, compared with acetal homopolymer.Acetal co-polymer is well-balanced in terms of mechanical, chemical and thermal properties, and its superior moldability allows it to be widely employed in various industrial fields.Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 144 MPa
20900 psi
ISO 527-1, 2
Elongation at Break 1.5 %
1.5 %
ISO 527-1, 2
Tensile Modulus 14.0 GPa
2030 ksi
ISO 527-1, 2
Flexural Strength 205 MPa
29700 psi
ISO 178
Flexural Modulus 12.0 GPa
1740 ksi
ISO 178
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 10.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
5.56 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 163 °C
325 °F
ISO 75-1, 2
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 300 ohm-cm
300 ohm-cm
IEC 60093
Surface Resistance 100 ohm
100 ohm
IEC 60093
Users viewing this material also viewed the following: