Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.0 GPa | 2030 ksi | ASTM D638 |
Premix Premi-Glas® 1100-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-10 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ASTM D638 |
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ASTM D638 |
Premix Premi-Glas® 1100-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-20 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ASTM D638 |
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ASTM D638 |
Premix Premi-Glas® 2207-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Tensile Modulus | 14.0 GPa @Temperature 23.0 °C |
2030 ksi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
(discontinu Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | 1 mm/min; ISO 527 - 1/2 |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ASTM D638 |
Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | |
LATI Laticonther 80 CPG/700 PPS, Glass Fiber Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Special filler. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ISO 527-1, 2 |
Polyplastics Duracon® CH-20 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ISO 527-1 |
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic Novolac resin based, glass fiber and glass beads reinforced. Very easy to transform in complex shapes. Excellent mechanical and thermal properties. Higher isotropic properties and good dimensional s.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ISO 527-1/-2 |
DSM Stanyl® TS256F8 Nylon 46-40% Glass Reinforced (Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-4H nat PA*-GF40 Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50 Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® RE15022 NC010 Polyethylene Terephthalate (PET) 36% Glass Reinforced Polyethylene TerephthalateRynite RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performan.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66
(Unverified Data**) 43% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G43HSLA BK099 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ISO 527 |
Eurotec® Tecomid® NB40 GR50 NL IL PA6, 50% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA black 9225 is a 40 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Tensile Modulus | 14.0 GPa @Temperature 70.0 °C, Time 720000 sec |
2030 ksi @Temperature 158 °F, Time 200 hour |
62% RH |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | ISO 527-1 |
Vyncolit W5020 Glass Filled Novolac Phenolic Novolac resin based, glass fiber and glass bead reinforced. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in the ABS system.Inform.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-4 FWA nat PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA natural is a 40 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Tensile Modulus | 14.0 GPa | 2030 ksi | |
LATI Latiohm 75/4-03 PD01 G/20 PBT, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |