Taiwan PU Corporation TPUI-G98 High Wear Resistance, Injection Molding Polycaprolactone Base TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer Taiwan PU Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPUI-G98 High Wear Resistance, Injection Molding Polycaprolactone Base TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
Tensile Strength at Break 44.13 MPa
6401 psi
Elongation at Break 550 %
550 %
100% Modulus 0.0127 GPa
1.84 ksi
300% Modulus 0.0206 GPa
2.99 ksi
Resilience 65
65
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 6.0
6.0
Processing Properties Metric English Comments
Feed Temperature 195 °C
383 °F
Middle Barrel Temperature 200 °C
392 °F
Compress zone
Front Barrel Temperature 205 °C
401 °F
Metering zone
Adapter Temperature 210 °C
410 °F
Die Temperature 210 °C
410 °F