Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 144.1 MPa | 20900 psi | ASTM D638 |
Plenco 50030 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup.. |
|||
Tensile Strength, Ultimate | 144 MPa | 20900 psi | ISO 527-1, 2 |
Polyplastics Duracon® CH-20 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 144 MPa | 20900 psi | 5mm/min; ISO 527 |
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Conditioned) Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6. |