| Category | Polymer , Thermoplastic , Elastomer, TPE |
| Manufacturer | Nagtong Polymax |
| Trade Name | Maxelast® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Polymax® Maxelast® A9860 TPE, ABS/PC Overmold.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 60 @Time 10.0 sec |
60 @Time 0.00278 hour |
ASTM D2240 |
| Tensile Stress | 2.03 MPa @Strain 100 % |
294 psi @Strain 100 % |
ASTM D412 |
| 3.24 MPa @Strain 300 % |
470 psi @Strain 300 % |
ASTM D412 | |
| Tensile Strength, Yield | 8.00 MPa | 1160 psi | ASTM D412 |
| Elongation at Break | 760 % | 760 % | ASTM D412 |