Mechanical Properties Metric English Comments
Tensile Stress 2.03 MPa

@Strain 100 %
294 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® A9860 TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Stress 2.03 MPa

@Strain 300 %,
Temperature 23.0 °C
294 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ CL2242 Thermoplastic Elastomer (TPE)
Versaflex™ CL2242 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov..
Tensile Stress 2.03 MPa

@Strain 300 %,
Temperature 23.0 °C
294 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 2.03 MPa

@Strain 300 %,
Temperature 23.0 °C
294 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion..
Tensile Stress 2.03 MPa

@Strain 300 %,
Temperature 23.0 °C
294 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7940-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7940-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 2.03 MPa

@Strain 300 %,
Temperature 23.0 °C
294 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7940-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7940-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion..
Tensile Stress 2.03 MPa

@Strain 67.88 %,
Temperature 100 °C
294 psi

@Strain 67.88 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 2.03 MPa

@Strain 67.88 %,
Temperature 100 °C
294 psi

@Strain 67.88 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers