ExxonMobil Exxtral™ BMU 130 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ BMU 130 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Europe Features:Balanced Stiffness/ToughnessDuctileGood UV ResistanceGood Weather ResistanceHigh Impact ResistanceLow Temperature Impact ResistanceUses: Automotive BumperAutomotive Exterior PartsAutomotive TrimProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 11.6 MPa
1680 psi
ISO 527-2
Tensile Strength, Yield 15.1 MPa
2190 psi
ISO 527-2
Elongation at Break 79 %
79 %
ISO 527-2
Elongation at Yield 4.3 %
4.3 %
ISO 527-2
Tensile Modulus 1.20 GPa
174 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.798 J/cm²

@Temperature -30.0 °C
3.80 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
1.09 J/cm²

@Temperature -20.0 °C
5.20 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
6.51 J/cm²

@Temperature 22.8 °C
31.0 ft-lb/in²

@Temperature 73.0 °F
Partial Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 47.2 °C
117 °F
ASTM D648
Users viewing this material also viewed the following: