Material Notes:
Information provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Water Absorption 0.10 %

@Thickness 0.508 mm
0.10 %

@Thickness 0.0200 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 43.0 MPa
6240 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
69.57 MPa
10090 psi
Type 1 - Rigids, 0.2 in/min, 50% in/in; ASTM D638
Elongation at Break 1.6 %
1.6 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 0.848 GPa
123 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 68.40 MPa
9921 psi
ASTM D790
Flexural Modulus 5.52 GPa
800 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.500 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity >= 2.02 W/m-K
>= 14.0 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 143.0 °C
289.4 °F
Unannealed, 0.062 in bars; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 22000 ohm
22000 ohm
ASTM D257
Descriptive Properties Value Comments
Product Form Pellets
Users viewing this material also viewed the following: