Polymer Property : Surface Resistivity per Square = 22000 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 22000 ohm
22000 ohm
ASTM D257
PolyOne Therma-Tech™ NJC-5000 TC NATURAL Nylon 12  (discontinued **)
Information provided by PolyOne Corporation.
Surface Resistivity per Square 22000 ohm
22000 ohm
ASTM D257
PolyOne Therma-Tech™ NJC-6500 Nylon 12  (discontinued **)
PolyOne First ChoiceInformation provided by PolyOne Corporation.