PolyOne Nymax™ 1010 A Natural Polyamide 6 (Nylon 6)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer PolyOne Corporation
Trade Name Nymax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Nymax™ 1010 A Natural Polyamide 6 (Nylon 6).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of fillers, glass reinforcement levels, and impact modifiers depending upon grade selected and have been formulated to offer ease of processing in most standard thermoplastic processing equipment.Molded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Water Absorption 1.0 %

@Thickness 3.18 mm
1.0 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 53.1 MPa
7700 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 140 %
140 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 68.9 MPa
9990 psi
ASTM D790
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Izod Impact, Notched 2.10 J/cm

@Thickness 3.18 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
Injection Molded; ASTM D256A
10.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
18.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 100 °C

@Thickness 3.18 mm
212 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C

@Thickness 3.18 mm
131 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Additive Impact Modifier
Appearance Natural Color
Features General Purpose
Impact Modified
Forms Pellets
Generic Material Nylon 6
Generic Name Polyamide 6 (Nylon 6)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Copyright © lookpolymers.com All Rights Reserved