Mechanical Properties Metric English Comments
Izod Impact, Notched 2.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
3.93 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87727-0284 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples. Physical property testing was based on the Geon® 87727 Trans 0020.Information provided by PolyOne
Izod Impact, Notched 2.10 J/cm

@Thickness 3.18 mm,
Temperature -18.0 °C
3.93 ft-lb/in

@Thickness 0.125 in,
Temperature -0.400 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 2.10 J/cm

@Thickness 3.18 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ 1010 A Natural Polyamide 6 (Nylon 6)
The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of ..
Izod Impact, Notched 2.10 J/cm

@Temperature 23.0 °C
3.93 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWM206 ASA
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.10 J/cm

@Temperature 23.0 °C
3.93 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWM206 ASA (Asia Pacific)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Asia Pacific regio..
Izod Impact, Notched 2.10 J/cm

@Temperature 23.0 °C
3.93 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Izod Impact, Notched 2.10 J/cm

@Thickness 3.18 mm,
Temperature -20.0 °C
3.93 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)
Information provided by Solvay Specialty Polymers.
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 300DA Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Information provided by Solvay Specialty Polymers.
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (discontinued **)
Information provided by Solvay Specialty Polymers.
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Information provided by Solvay Specialty Polymers.
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Powder grades for masterbatches.Information provided by Solvay Specialty Polymers.
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Information provided by Solvay Specialty Polymers.
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 513LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Information provided by Solvay Specialty Polymers.
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 901 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)<
Information provided by Solvay Specialty Polymers.
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)<
Information provided by Solvay Specialty Polymers.
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 1450LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polyme..
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 300DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Features: Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 ..
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 350LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol..
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0..
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov..
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 513LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityUses: MonofilamentsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solv..
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 930LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol..
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol..
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym..
Izod Impact, Notched 2.10 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 902 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 28.0 J/g; Heat of Fusion - ASTM D3418 28.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym..
Izod Impact, Notched 2.10 J/cm

@Temperature 23.0 °C
3.93 ft-lb/in

@Temperature 73.4 °F
Practical Use (Water Absorption 1.7%); ASTM-D256
Toyobo GLAMIDE® T-602G30 MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 2.10 J/cm

@Temperature 23.0 °C
3.93 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)  (discontinued **)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..