Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M3890 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M4805 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790 |
PolyOne Gravi-Tech™ GRV-NJ-110-W Polyamide 12 (Nylon 12) Information provided by PolyOne |
|||
Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790 |
PolyOne Gravi-Tech™ GRV-PS-027-BA-WHT Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790 |
PolyOne Nymax™ 1010 A Black 13 Polyamide 6 (Nylon 6) The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of .. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790 |
PolyOne Nymax™ 1010 A Natural Polyamide 6 (Nylon 6) The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of .. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NX9270 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NX9294 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NX9300 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NX9320 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NY9208 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NY9217 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NY9220 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | Crosswise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NY9233 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | |
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance S-679 is an isostatically pressed graphite material that is treated to provide oxidation resistance at elevated temperatures. This material performs well in glass contact applications where heat an.. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | 13 mm/min; ASTM D790 |
PolyOne Edgetek® X AS/018 White Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790 |
PolyOne Edgetek® AT-000/000 HI5 Natural NA Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790M |
DSM Somos® 14120 Water-resistant resin for stereolithography, White DescriptionDSM Somos® 14120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant parts. Parts created with Somos® 14120 have a white, opaque appearance similar to p.. |
|||
Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M4820 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 68.9 MPa | 9990 psi | ASTM D790 |
PolyOne Edgetek® XT XT-100-CX02-EG PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |