Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.013 - 0.015 cm/cm
0.013 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
15 sec; ASTM D2240
85
85
ASTM D2240
Tensile Strength at Break 16.2 MPa
2350 psi
510 mm/min; ASTM D638
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 400 %
400 %
510 mm/min; ASTM D638
Tear Strength 70.1 kN/m
400 pli
Die C, 510 mm/min; ASTM D624
Compression Set 28 %

@Temperature 23.0 °C,
Time 79200 sec
28 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.331 GPa
48.0 ksi
ASTM D1043
0.310 GPa

@Temperature -32.0 °C
45.0 ksi

@Temperature -25.6 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -36.1 °C
-33.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 174 - 179 °C
345 - 354 °F
188 - 199 °C
370 - 390 °F
Descriptive Properties Value Comments
Features General Purpose
Medium Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose