Material Notes:
Automotive OEM approval(s).Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
15 sec; ASTM D2240
70
70
ASTM D2240
Tensile Strength at Break 10.5 MPa
1520 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 380 %
380 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 31.5 kN/m
180 pli
Die C, 510 mm/min; ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Flame Spread 0.00 mm/min
0.00 in/min
Automotive Burn Test; FMVSS 302
Descriptive Properties Value Comments
Cold Flexibility Pass
GM 9503P; -29°C, 1.91 mm; 25 mm, 4 hr
Features Low Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Interior Trim
Xenon Weatherometer Pass
SAE J1960; Interior, 602 kJ/m², All Colors, dE*<3.0