Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable JG513G2 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable WJLC32L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible 90461 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible XV3440 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Teknor Apex APEX® 3200-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Teknor Apex APEX® 3600-70NT Polyvinyl Chloride, Flexible
Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: First Generation SeriesInformation Provided by Teknor Apex
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Teknor Apex APEX® 3700-60 Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Teknor Apex APEX® 3800-60 Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor ..
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Teknor Apex APEX® 07-U0296B-80 Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Teknor Apex APEX® 3300-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me..
Brittleness Temperature -44.0 °C
-47.2 °F
Sylvin Technologies 5134-70 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Brittleness Temperature -44.0 °C
-47.2 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Control Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Brittleness Temperature -44.0 °C
-47.2 °F
Temperature Retraction, TR-10
Dow Nordel® IP 4520 General Purpose Compound
FormulationNordel® IP 4520
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Colorite Polymers 6500 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Colorite Polymers 6507 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Brittleness Temperature -44.0 °C
-47.2 °F
Colorite Polymers 6511 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
Brittleness Temperature -44.0 °C
-47.2 °F
Colorite Polymers 6512 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..
Brittleness Temperature -44.0 °C
-47.2 °F
Colorite Polymers Self Frosting™ 6511SF Vinyl Compound
Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi..
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer
Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Brittleness Temperature -44.0 °C
-47.2 °F
Impact Brittleness; ASTM D746
Bayshore Vinyl Compounds BVC 1100-65 Clear PVC Compound
BVC 1100-65 is a clear flexible PVC compound produced with FDA sanctioned ingredients. It is recommended for use in applications for the medical, food and beverage industries. This material offers..
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D-746
Axiall 12770 Coax & Telecom Flexible PVC
Non-lead stabilized, CATV and general purpose jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D-746
Axiall 16860 Wire & Cable Flexible PVC
Battery booster jacket compound and general purpose jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D 746
AlphaGary Evoprene™ LF 6158 Automotive Thermoplastic Elastomer
Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab..
Brittleness Temperature -44.0 °C
-47.2 °F
AlphaGary Garaflex™ E 4832 Natural UV LCF Vinyl Thermoplastic Elastomer
Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cableA lead free, up resistant, flame retarded, oil resistant compound designed for wind turbine jacket applications
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Teknor Apex APEX® 2570-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Brittleness Temperature -44.0 °C
-47.2 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Control Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Alliance Polymers Zythane™ 4070A Thermoplastic Polyurethane Elastomer
Zythane™ 4070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Brittleness Temperature -44.0 °C
-47.2 °F
Sylvin Technologies 5123 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Brittleness Temperature -44.0 °C
-47.2 °F
Cold Flex; ISO 458/2
Fainplast Compounds CL 62 Flexible PVC, Sheathing
Sheath various purposes good flexibility
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D-746
Axiall 38602 Coax & Telecom Flexible PVC
CATV and general purpose jacket with excellent low temperature properties. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axial..