Thermal Properties Metric English Comments
Flame Spread 0.00 mm/min
0.00 in/min
Automotive Burn Test; FMVSS 302
PolyOne Geon™ Vinyl Flexible 90401 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Flame Spread 0.00 mm/min
0.00 in/min
Automotive Burn Test; FMVSS 302
PolyOne Geon™ Vinyl Flexible 90450 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Flame Spread 0.00 mm/min
0.00 in/min
Automotive Burn Test; FMVSS 302
PolyOne Geon™ Vinyl Flexible 90451 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Flame Spread 0.00 mm/min
0.00 in/min
Automotive Burn Test; FMVSS 302
PolyOne Geon™ Vinyl Flexible 90461 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Flame Spread 0.00 mm/min
0.00 in/min
Automotive Burn Test; FMVSS 302
PolyOne Geon™ Vinyl Flexible R295AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Flame Spread 0.00 mm/min
0.00 in/min
FMVSS302
Azdel Plus C467-B01 45% Chopped Fiber Mat / PP Resin Matrix (Mineral filled)
AZDEL® C467-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu..