Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.5 MPa | 1520 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 90250 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.5 MPa | 1520 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 90461 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tensile Strength at Break | 10.5 MPa | 1520 psi | Type IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638 |
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Tensile Strength at Break | 10.5 MPa | 1520 psi | ASTM D638 |
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade Description: The physical and structural characteristics of LUTENE MB9500 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Powder coating, artific.. |
|||
Tensile Strength at Break | <= 10.5 MPa | <= 1520 psi | after aging (6 weeks); IEC 60811-1-2 |
Borealis Visico™/Ambicat™ LE4427/LE4476 Polyethylene Compound, Crosslinkable Visico™ LE4427 / Ambicat™ LE4476 is a silane crosslinkable black compound designed for weather resistant covering/insulation of overhead and façade cables. The black base material Visico™ LE442.. |
|||
Tensile Strength at Break | 10.5 MPa | 1520 psi | ISO 527-2 |
Carmel Olefins IPETHENE® 670 Low Density Polyethylene IPETHENE® 670 is a low density polyethylene extrusion coating and lamination grade. This grade can be processed at high coating temperatures and coating speeds. It exhibits low neck-in and stable w.. |
|||
Tensile Strength at Break | 10.5 MPa | 1520 psi | ISO 527-2 |
Carmel Olefins IPETHENE® 810 Low Density Polyethylene IPETHENE® 810 is a low density polyethylene injection molding grade. It exhibits high melt flow rate, high gloss, and high stiffness. APPLICATIONS IPETHENE® 810 is used to produce lids, containe.. |
|||
Tensile Strength at Break | 10.5 MPa | 1520 psi | ISO 527-2 |
Carmel Olefins IPETHENE® 470 Low Density Polyethylene IPETHENE® 470 is a low density polyethylene extrusion coating and lamination grade. This grade can be processed at high coating temperatures and coating speeds. It exhibits low neck-in and stable w.. |
|||
Tensile Strength at Break | 10.5 MPa | 1520 psi | ISO 527-2 |
Carmel Olefins IPETHENE® 600 Low Density Polyethylene IPETHENE® 600 is a low density polyethylene injection molding grade. This grade is a good carrier for masterbatches production. It exhibits good stiffness and moderate melt flow rate. APPLICATIONS.. |
|||
Tensile Strength at Break | <= 10.5 MPa | <= 1520 psi | after aging 168h, 150°C, 9% catalyst); IEC 60811-1-2 |
Borealis Visico™/Ambicat™ LE4421/LE4476 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4476 is a silane crosslinkable natural compound designed for low voltage power cables up to 6kV. The base material Visico™ LE4421 in combination with the catalyst mas.. |