Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucas-Milhaupt Silvaloy® A54N Brazing Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Silvaloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Silvaloy® A54N Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silvaloy A54N is a silver brazing alloy suitable for furnace brazing due to its low zinc content. Its broader melting range is helpful where clearances are not uniform. During melting, Silvaloy A54N passes from the solid state to a mushy or plastic state and progressively to a liquid. Typical applications are the joining of ferrous, non-ferrous, and dissimilar metals and alloys.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 9.63 g/cc
9.63 g/cc
Density 9.62 g/cc
0.348 lb/in³
Thermal Properties Metric English Comments
Melting Point 718.3 - 857.2 °C
1325 - 1575 °F
Solidus 718.3 °C
1325 °F
Liquidus 857.2 °C
1575 °F
Maximum Service Temperature, Air 371 °C
700 °F
Component Elements Properties Metric English Comments
Copper, Cu 39 - 41 %
39 - 41 %
Nickel, Ni 0.50 - 1.5 %
0.50 - 1.5 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 53 - 55 %
53 - 55 %
Zinc, Zn 4.0 - 6.0 %
4.0 - 6.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000346 ohm-cm
0.00000346 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 857.2 - 968.3 °C
1575 - 1775 °F
Brazing Temperature
Descriptive Properties Value Comments
Color White
Electrical Conductivity (% IACS) 49.8