Mechanical Properties Metric English Comments
Tensile Stress 6.14 MPa

@Strain 100 %
891 psi

@Strain 100 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2155 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..
Tensile Stress 6.14 MPa

@Strain 50.0 %
891 psi

@Strain 50.0 %
Average; ASTM D412 Method A
Seals Eastern 7042U Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..
Tensile Stress 6.14 MPa

@Strain 0.250 %,
Temperature 160 °C
891 psi

@Strain 0.250 %,
Temperature 320 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..