Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 19.3 kN/m | 110 pli | ASTM D412 |
Multibase TPSiV™ 3340-65A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | ASTM D624 |
Network Polymers Softflex® 0250 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 19.3 kN/m | 110 pli | ASTM D624 |
PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2712-1000-02 is an easy processing TPE designed for injection molding and extrusion aplications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - High.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ XL-2155 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible 82024 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 19.3 kN/m | 110 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 5521 BLK TPE A 5521 is based on Shell's Kraton technology licensed to Multibase. The product is extensively used in automotive and non-automotive applications. Multi-Flex TPE contains Kraton™ G.Data p.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | Die B,molded-without post cure; ASTM D624 |
Multibase C6-235 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 19.3 kN/m | 110 pli | ASTM D624 |
Multibase Multi-Flex® A 5001 E LC Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase |
|||
Tear Strength | 19.3 kN/m | 110 pli | Die C; ASTM D624 |
Teknor Apex Flexalloy® 9100-35 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | Die C; ASTM D624 |
Teknor Apex Monprene® MP-2815B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-1522E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tear Strength | 19.3 kN/m | 110 pli | ASTM D624 |
Teknor Apex UNIPRENE® 7010-55 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 19.3 kN/m | 110 pli | Trouser; ASTM D470 |
Lubrizol Estane® MVT 75AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 75AT3 is a 75A aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | ASTM D624 |
Teknor Apex Uniprene® UN-7010-55NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | |
Dow Corning HS III BASE & 10:1 COLORED CATALYST High strength lower durometer silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items. HS III Base with HS III 10:1 Colored Catalyst is recommended.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | |
Dow Corning HS III HS SPRAYABLE CATALYST - CLEAR High strength lower durometer silicone mold making rubber, suited for the reproduction of robotic skins, tooling and immovable objects due to its thixotropic characteristics. HS III Base with HS Spr.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | |
Dow Corning SILASTIC® LS 4-9062 FLUOROSILICONE RUBBER 65 durometer, off-white, uncatalysed, fluorosilicone base.Information provided by Dow Corning |
|||
Tear Strength | 19.3 kN/m | 110 pli | |
Dow Corning 5-8601 FLUOROSILICONE LSR, KIT Fluorosilicone rubber designed for liquid injection moldingInformation provided by Dow Corning |
|||
Tear Strength | >= 19.3 kN/m | >= 110 pli | Die B |
Aremco EZ-Cast™ 580N Silicon Molding Compound Silicone Rubber Aremco's EZ-Cast™ 580N is an ideal compound for producing high reliability master molds. This silicone rubber compound exhibits high tear strength, very low shrinkage and high flexibility, all requ.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | cured 72 hrs@ RT |
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Tear Strength | 19.3 kN/m | 110 pli | die B; ASTM D624 |
R70-068 Styrene-based Biomedical Elastomer |