PolyOne Edgetek® PI-20GF/000 Polyetherimide (PEI), Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® PI-20GF/000 Polyetherimide (PEI), Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Water Absorption 0.22 %

@Thickness 3.17 mm
0.22 %

@Thickness 0.125 in
24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 148 MPa
21500 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Elongation at Break 4.0 - 5.0 %
4.0 - 5.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 360 - 399 °C
680 - 750 °F
Molding