PolyOne Edgetek® NJ-30GF/000 Nylon 12, Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® NJ-30GF/000 Nylon 12, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.234 g/cc
1.234 g/cc
ASTM D792
Water Absorption 0.25 %

@Thickness 3.17 mm
0.25 %

@Thickness 0.125 in
24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 117 MPa
17000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 6.89 GPa
1000 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 1.82 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
3.40 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 177 °C
350 °F
Unannealed, 0.125 in bars; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Unannealed, 0.125 in bars; ASTM D648