Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
PolyOne Edgetek® NJ-30GF/000 Nylon 12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
PolyOne Therma-Tech™ NJC-6500 Nylon 12
(discontinued **) PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | Compression; ASTM D955 |
Plenco 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | Compression; ASTM D955 |
Plaslok 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 308 is a two-stage, mineral and flock.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | Compression; ASTM D955 |
Plaslok 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® 155D S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® 160D S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® L185A Polycaprolactone Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® X595A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | |
Styron Pulse® 1550 ABS + Polycarbonate, 10% Glass Reinforced PULSE® 1550 Engineering resin is a 10% glass reinforced resin which offers a superior total performance with a balance of high heat resistance, practical toughness and ease of processing.Data pro.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | RHODIA-EP |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Linear Mold Shrinkage | 0.0045 - 0.0055 cm/cm | 0.0045 - 0.0055 in/in | |
Polyram PlusTek PA301G3 Nylon 6.6, Heat Stabilized, 15% Glass Fiber Heat stabilized, 15% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0045 - 0.0055 cm/cm | 0.0045 - 0.0055 in/in | |
Polyram PlusTek RA303G4 Nylon 6.6, 20% Glass Fiber 20% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0045 - 0.0055 cm/cm | 0.0045 - 0.0055 in/in | |
Polyram PlusTek RA307G4 Nylon 6.6, 20% Glass Fiber 20% glass fiber reinforced heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
Adell AR-34 Nylon 66, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
Adell BR-34 Nylon 6, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | restricted |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | restricted |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
Ashley Polymers Ashlene® 528L-40G Nylon 66, 40% Glass Reinforced A general purpose 40% glass reinforced Nylon 66 resin.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.0045 - 0.0055 cm/cm | 0.0045 - 0.0055 in/in | IS 13411-1992 |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
Adell AR-14 Nylon 66, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | restricted |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | restricted |
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® 195A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |