Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.234 g/cc | 1.234 g/cc | ASTM D792 |
PolyOne Edgetek® NJ-30GF/000 Nylon 12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |