Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Polymer Resources PCSF-FRG30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade Polycarbonate, 30% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
LNP Lubricomp® OFL-4536 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire PEEK is produced to the .. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
LNP Thermocomp® GF-1006 Polysulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
PolyOne Lubri-Tech™ SF-25GF/13T BLACK Polyphenylene Sulfide (PPS), Glass Filled, PTFE Lubricated
(discontinue Description/Features:Glass Fiber ReinforcedPTFE LubricatedBlackPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Kotec Carbotex KG-20MRA Polycarbonate, 20% Glass Fiber Reinforced Features: Glass fiber 20% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES Electrablend® PA12 CF13 L 13% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 13% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and lubricatedInformation provided by TP Composi.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK) KetaSpire® KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industr.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK) KetaSpire® KT-880P is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standard.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF/B40 L 40% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 40% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: Natural ColorInformation provided by TP.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF10 L BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 0135 BL069 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF/M40 IG BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES HiFill® PET GF20 UV BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: UV StabilizerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES Statiblend® PA6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Antistatic, Heat Stabilizer and LubricantFeatures: Antistatic, Heat Stabilizer and Lubricate.. |
|||
Flexural Strength | 152 MPa | 22000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX8410W PPE+PA High flow, 10% Glass Reinforced PPE+PA. Typically used in Automotive connectors. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Chase Plastics CP Pryme® N310L (Dry) Nylon 6, 10% Glass Fiber Reinforced, Lubricated, Recycled Content Features: LubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 630 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing .. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
PolyOne Edgetek® ES-10GF/000 PES (Polyethersulfone), 10% Glass Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
SABIC Innovative Plastics NORYL CN5246 PPE+PS (Asia Pacific) |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF15 FR BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
PolyOne Lubri-Tech™ PS-30GF/10T2S Polybutylene Terephthalate (PBT), Glass Filled, PTFE/Silicone Lubricated
(d Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |