Material Notes:
Moplen EP300H is a heterophasic copolymer, suitable for injection moulding as well as for thermoforming applications. Moplen EP300H is a excellent low temperature impact behavior combined with a good processability. Moplen EP300H is suitable for food contact. Features: High impact strength at low temperature/Optimized balance of stiffness and toughness/High surface hardness/Good dimensional stability/Good pigment dispersion/Lower warpageApplications: Houseware/Crates/Stackable boxes/Small Appliances/Toy articles /Thermoforming applications/Margarine tubs/Ring balance in WM /Stationary sheets/Blow molding bottles/Pail lidsInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 27.5 MPa
3980 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.08 GPa
156 ksi
ASTM D790
Izod Impact, Notched 0.588 J/cm

@Temperature -20.0 °C
1.10 ft-lb/in

@Temperature -4.00 °F
ASTM D256
4.90 J/cm

@Temperature 23.0 °C
9.18 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648