Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeros Mexicanos Rotolene® Natural Linear Medium Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer Polimeros Mexicanos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeros Mexicanos Rotolene® Natural Linear Medium Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized. Available as natural and several colors powder compounds.High quality Polyethylene recommended for general purpose applications. Frequently used for water tanks and small to medium size containers exhibiting very good mechanical properties. When used for inner layers, it provides excellent smooth finish and texture.Natural Resin, which is used as a carrier in color compounds meets all requirements of US food and drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Information provided by Polimeros Mexicanos
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
ASTM D1693
ESCR 10% Igepal® >= 200 hour
>= 200 hour
ASTM D1693
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
2 in/min; ASTM D638
Tensile Strength, Yield 18.6 MPa
2700 psi
2 in/min; ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 0.689 GPa
100 ksi
1% Secant; ASTM D790
Impact Test 67.8 J

@Temperature -40.0 °C
50.0 ft-lb

@Temperature -40.0 °F
0.125 in.; ARM STD test
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ASTM D648
Descriptive Properties Value Comments
Process Rotational Molding
Region Europe/Turkey
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved