| Category | Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS) |
| Manufacturer | Polimeri Europa (Former EniChem) |
| Trade Name | Europrene® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Polimeri Europa Europrene® SOL T 166 Styrene - Butadiene Block Copolymer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
| Brookfield Viscosity | 0.13 cP | 0.13 cP | Toluene sol., 25% wt; ASTM D1084 |
| Melt Flow | 6.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
6.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 72 | 72 | ASTM D2240 |
| Tensile Strength at Break | 20.0 MPa | 2900 psi | ASTM D412 |
| Elongation at Break | 800 % | 800 % | ASTM D412 |
| 300% Modulus | 0.00250 GPa | 0.363 ksi | ASTM D412 |