Material Notes:
NanoActive CaO Plus is produced using proprietary processes to obtain high specific surface area (over 90 m²/g vs. 1-2 m²/g for standard CaO), small crystallite size material possessing high chemical reactivity towards many chemical hazards including carbon dioxide and hydrogen sulfide.Applications: Applications include desiccant, destruction of chemical warfare agents, elevated temperature hazardous waste treatment, flue gas treatment, insecticide and fungicide, odor reduction, precursor, pulp and paper, and water treatment.Information provided by NanoScaleComposition based on metal
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
Density 3.10 g/cc
0.112 lb/in³
Particle Size 4.0 µm
4.0 µm
mean aggregate size
Specific Surface Area >= 90 m²/g
>= 90 m²/g
BET
Pore Size 0.0110 microns
0.000433 mil
Average Diameter
Component Elements Properties Metric English Comments
Calcium, Ca >= 99.4 %
>= 99.4 %
Descriptive Properties Value Comments
Appearance / Color White Powder
Crystallite Size = 20 nm
Minimum Total Pore Volume cc/g 0.2
Users viewing this material also viewed the following: