Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastics Group Polifil® 930L Nylon 6 (DAM)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® 930L Nylon 6 (DAM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® NYLON 6 provides superior strength and rigidity with electrical resistance and surface lubricity.Applications: AutomotiveHousingsBearingsAppliances Standard processing techniques are applicable. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.6 %
1.6 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 3.17 mm
0.012 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 2.69 GPa
390 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
420 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C
145 °F
ASTM D648