Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastiComp Velocity® LGF60-PA6 High Flow Nylon 6, 60% Long Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 60% Glass Fiber Filled
Manufacturer PlastiComp
Trade Name Velocity®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Velocity® LGF60-PA6 High Flow Nylon 6, 60% Long Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.69 g/cc
1.69 g/cc
ASTM D-792
Filler Content 60 %
60 %
Long Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength 255 MPa
37000 psi
ASTM D-638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D-638
Tensile Modulus 20.0 GPa
2900 ksi
ASTM D-638
Flexural Strength 407 MPa
59000 psi
ASTM D-790
Flexural Modulus 17.24 GPa
2500 ksi
ASTM D-790
Izod Impact, Notched 3.20 J/cm
5.99 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 12.8 J/cm
24.0 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
ASTM D-648
Users viewing this material also viewed the following: