Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D-790 |
PlastiComp Complet® LCF15/LGF35 – PA66 BLK Polyamide 66, 50% Long Carbon/Glass Fiber Composite PelletsInformation provided by PlastiComp, Inc. |
|||
Flexural Modulus | 17.24 GPa | 2500 ksi | ASTM D-790 |
PlastiComp Velocity® LGF60-PA6 High Flow Nylon 6, 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Oxford Polymers 30CF 30% Carbon Fiber Reinforced Polyphenylene Sulfide 30% Carbon Fiber Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 17.2 GPa @Temperature 23.9 °C |
2500 ksi @Temperature 75.0 °F |
Dry; 325°F, 1000psi Cured; ASTM D790 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, Silica Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PS-30CF/10T 2S Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced, PTFE/Silicone Lubricated Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
PolyOne Edgetek® PK-20CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
PolyOne Edgetek® PK-30CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCN3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | |
MTI ThermoStran® PA66-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Techmer ES Electrafil® J-3/CF/30 Nylon 6, 30% Carbon Fiber Reinforced |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Techmer ES Luriblend® PEI CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Clariant Renol PPA1100G50 Polyphthalamide, 50% Glass Fiber Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 17.2 - 19.3 GPa | 2500 - 2800 ksi | Average value: 18.1 GPa Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% .. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
PolyOne Edgetek® PI-30CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |