Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D-792 |
PlastiComp Velocity® LGF60-PA6 High Flow Nylon 6, 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D-792 |
PlastiComp Velocity® LGF60-PA66 High Flow Nylon 66, 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
Ovation Polymers Nima™ HL 30530 GF FR PET, 30% Glass Fiber PET – Flame Retardant 30% Short Glass Fiber Reinforced. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM s.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | Method A; ASTM D792 |
LNP Lubricomp® OFL-4036 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
LG Chemical LUMID HM2604AW PA6+GF60% Feature: Injection Molding, PA6+GF60%Application: Bath liftInformation provided by LG Chemical |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | |
Lord Adhesives Thermosetâ„¢ ME-455-1 Epoxy Board Level Encapsulant LORD Thermosetâ„¢ ME-455-1 encapsulant is a low viscosity, one-component, semiconductor grade epoxy designed for the encapsulation of wire-bonded or flip chip die in PPGA, BGA, MCM and other cavi.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ISO 1183 |
Lanxess Pocan® ECO T 3240 000000 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, contains 25% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | |
Silberline Silvet® 460-30-E1 Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final processi.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ 60186U Almond Concentrate Based in LLDPE DescriptionPOLYBATCH® Almond 60186U is an almond color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. POLYBATCH® 60186U is heavy metal free and is typically.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
A. Schulman PAPERMATCH® T-4228-8 Specialty Masterbatch DescriptionPAPERMATCH® T-4228-8 is a specialty masterbatch formulated to impart paper-like properties to polyethylene films. PAPERMATCH® T-4228-8 is a white, medium opacity grade designed to prov.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ 60186U Almond Concentrate Based in LLDPE DescriptionPOLYBATCH® Almond 60186U is an almond color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. POLYBATCH® 60186U is heavy metal free and is typically.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ 60186U Almond Concentrate Based in LLDPE DescriptionPOLYBATCH® Almond 60186U is an almond color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. POLYBATCH® 60186U is heavy metal free and is typically.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ 60186U Almond Concentrate Based in LLDPE DescriptionPOLYBATCH® Almond 60186U is an almond color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. POLYBATCH® 60186U is heavy metal free and is typically.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
A. Schulman PAPERMATCH® T-4228-8 Specialty Masterbatch DescriptionPAPERMATCH® T-4228-8 is a specialty masterbatch formulated to impart paper-like properties to polyethylene films. PAPERMATCH® T-4228-8 is a white, medium opacity grade designed to prov.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
A. Schulman PAPERMATCH® T-4228-8 Specialty Masterbatch DescriptionPAPERMATCH® T-4228-8 is a specialty masterbatch formulated to impart paper-like properties to polyethylene films. PAPERMATCH® T-4228-8 is a white, medium opacity grade designed to prov.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
A. Schulman PAPERMATCH® T-4228-8 Specialty Masterbatch DescriptionPAPERMATCH® T-4228-8 is a specialty masterbatch formulated to impart paper-like properties to polyethylene films. PAPERMATCH® T-4228-8 is a white, medium opacity grade designed to prov.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | |
BCC Products BC 7136 Epoxy Casting BC7136 is a gray, low toxicity, aluminum filled, epoxy casting resin. This heat resistant system may be used at room temperature without post-curing. May be cast to a thickness of ¾ inch in non-con.. |
|||
Specific Gravity | 1.69 g/cc | 1.69 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 LNP THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |