Polymer Property : Flexural Strength = 59000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 407 MPa
59000 psi
ASTM D-790
PlastiComp Complet® LGF60 - PA66 Nylon 66, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 60% long glass fiber reinforcementInformation provided by PlastiComp, In..
Flexural Strength 407 MPa
59000 psi
ASTM D-790
PlastiComp Velocity® LGF60-PA6 High Flow Nylon 6, 60% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Flexural Strength 407 MPa
59000 psi
ASTM D-790
PlastiComp Velocity® LGF60-PA66 High Flow Nylon 66, 60% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Flexural Strength 407 MPa
59000 psi
ASTM D790
Techmer ES Electrafil® J-1/CF/40 BK PA66
Flexural Strength 407 MPa
59000 psi
ASTM D790
Techmer ES Electrafil® J-1/CF/40 NAT PA66
Flexural Strength 407 MPa
59000 psi
ASTM D790
Techmer ES HiFill® PA6/6 LGF50 HS L BK 12 mm
Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Good MoldabilityUL File Number: E15731..
Flexural Strength 407 MPa
59000 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON RE006 PA6.6 (Asia Pacific)
LNP STAT-KON RE006 is a compound based on Nylon 66 containing carbon fiber. Added features of this material include: Electrically Conductive. Also known as STAT-KON RC-1006