Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Phillips 66 COPYLENE® CR750CLS Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Phillips 66
Trade Name COPYLENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Phillips 66 COPYLENE® CR750CLS Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: COPYLENE® CR750CLS is a clarified random copolymer specially designed and formulated for clear injection molding applications and is formulated with antistat and lube for excellent mold release and material handling.Applications: Injection MoldingInformation provided by Phillips 66.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 230 °C
75 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
(2 in/min); ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 1.03 GPa
150 ksi
0.05 in/mm, 1% Secant, Procedure A; ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
Method A; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved