Material Notes:
PERMABOND UV645 is a single part, fast curing, high viscosity UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbonate as well as metals and glass. Permabond UV645 has very high shear strength, elongation and impact resistance making it ideal for applications that require substrates with different coefficients of thermal expansion. Permabond UV645 has good depth of curing capabilities which make it suitable for use as a sealant. Protect liquid adhesive from room lighting. Features & Benefits: Cure on demand High shear strength Fast curing with low-power lamps 100% solids, no solvents Excellent adhesion to plastics Information provided by Permabond.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
uncured
Viscosity 10000 - 12000 cP

@Temperature 25.0 °C
10000 - 12000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Tensile Strength 11.0 MPa
1600 psi
ASTM D2095
Elongation at Break 110 %
110 %
Adhesive Bond Strength >= 5.00 MPa
>= 725 psi
PVC , Shear
>= 7.00 MPa
>= 1020 psi
PC to ABS, Shear
>= 9.00 MPa
>= 1310 psi
Polycarbonate, Shear
Optical Properties Metric English Comments
Refractive Index 1.47
1.47
Electrical Properties Metric English Comments
Dielectric Constant 4.0

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
4.0

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Dielectric Strength 12.0 kV/mm
305 kV/in
Processing Properties Metric English Comments
Cure Time 0.117 min
0.00194 hour
fixture time, (low power 4mW lamp)
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear, colorless
Uncured
Cure Wavelength (nm) 365-420
Maximum Gap Fill (mm) 0.5
Strength Retention 10% at 200°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 150°C
Relative to 0°C
75% at 100°C
Relative to 0°C
95% at 50°C
Relative to 0°C
Users viewing this material also viewed the following: