Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.117 min | 0.00194 hour | fixture time, (low power 4mW lamp) |
Permabond UV640 UV-curable Adhesive PERMABOND UV640 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Cure Time | 0.117 min | 0.00194 hour | fixture time, (low power 4mW lamp) |
Permabond UV645 UV-curable Adhesive PERMABOND UV645 is a single part, fast curing, high viscosity UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including .. |
|||
Cure Time | >= 0.117 min | >= 0.00194 hour | Fixture |
Resinlab® CYNERGY CA6601 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Cure Time | 0.117 min | 0.00194 hour | fixture time, (low power 4mW lamp) |
Permabond UV649 UV-curable Adhesive PERMABOND UV649 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Cure Time | 0.117 min | 0.00194 hour | fixture time, (low power 4mW lamp) |
Permabond UV670 UV-curable Adhesive PERMABOND UV670 is a single part, fast curing, UV curable adhesive. The cured adhesive is tough, flexible and has excellent impact resistance. Permabond UV670 is well suited for bonding glass to met.. |
|||
Cure Time | 0.117 - 0.167 min | 0.00194 - 0.00278 hour | PVC, handling time |
Permabond 102 Cyanoacrylate, General purpose PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano.. |
|||
Cure Time | 0.117 - 0.167 min | 0.00194 - 0.00278 hour | ABS, handling time |
Permabond 102 Cyanoacrylate, General purpose PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano.. |
|||
Cure Time | >= 0.117 min | >= 0.00194 hour | Fixture |
Resinlab® CYNERGY CA6701 Adhesive Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal .. |
|||
Cure Time | >= 0.117 min | >= 0.00194 hour | Fixture |
Resinlab® CYNERGY CA6901 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Cure Time | 0.117 min | 0.00194 hour | Hot tack |
Valley Adhesives EM-420 High Temperature Application Glue Stick Valley Adhesives EM-420 High Temperature Application Glue StickBonds many plastics, polyolefins and light weight materials. |
|||
Cure Time | 0.117 min | 0.00194 hour | Hot tack |
Valley Adhesives EM-600 High Temperature Application Glue Stick Valley Adhesives EM-600 High Temperature Application Glue StickBonds many woods and wood composites; Excellent for woodworking and cabinetry. |