Ovation Polymers Opnyl OP6GF33 Nylon 6, 33% Glass Reinforced, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Ovation Polymers
Trade Name Opnyl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Opnyl OP6GF33 Nylon 6, 33% Glass Reinforced, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6 - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the measurements are done in dry and wet conditions. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm

@Thickness 3.17 mm
0.0015 - 0.0025 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
50 mm/min; ASTM D638
Elongation at Break 5.5 %
5.5 %
50 mm/min; ASTM D638
Tensile Modulus 6.90 GPa
1000 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 170 MPa
24700 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5.40 GPa
783 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 1.255 J/cm
2.351 ft-lb/in
ASTM D256