Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.255 J/cm @Temperature 23.0 °C |
2.351 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers Opnyl OP66GF50 Nylon 66 Nylon 66-Glass reinforced(50%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers |
|||
Izod Impact, Notched | 1.255 J/cm | 2.351 ft-lb/in | ASTM D256 |
Ovation Polymers Opnyl OP6GF33 Nylon 6, 33% Glass Reinforced, Conditioned Nylon 6 - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |