Mechanical Properties Metric English Comments
Izod Impact, Notched 1.255 J/cm

@Temperature 23.0 °C
2.351 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Ovation Polymers Opnyl OP66GF50 Nylon 66
Nylon 66-Glass reinforced(50%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers
Izod Impact, Notched 1.255 J/cm
2.351 ft-lb/in
ASTM D256
Ovation Polymers Opnyl OP6GF33 Nylon 6, 33% Glass Reinforced, Conditioned
Nylon 6 - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m..