Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.90 GPa | 1000 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nemcon™ H PC DP105/X3 BK Polycarbonate Polycarbonate-Black colored, thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP6GF33 Nylon 6, 33% Glass Reinforced, Conditioned Nylon 6 - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | |
Reliance Industries PET - 35% Glass filled Information provided by Reliance Industries |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP CX05031 PS (Europe-Africa-Middle East) LNP* Lubricomp* CX05031 is a compound based on Polystyrene resin containing Graphite, Silicone. Added features include; Internally Lubricated. |
|||
Tensile Modulus | 6.90 GPa @Temperature 23.0 °C |
1000 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK603 BK851 PBT
(Unverified Data**) Crastin® SK603 BK851 is a 20% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ASTM D638 |
PolyOne Edgetek® ES-20GF-15GM/000 Polyethersulfone - 20% Glass Fiber - 15% Milled Glass
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | |
Reliance Industries PBT / PC - 35% Glass filled Information provided by Reliance Industries |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 3225 XF 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, improved flowability |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP (Europe-Africa-Middle East) LNP* Lubricomp* MFL36S is a compound based on Polypropylene resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, Conditioned Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors .. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Compression Grade Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Injection Grade Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | 1mm/min; ISO 527-2 |
Borealis GB364WG Polypropylene Compound, Glass Fiber Reinforced GB364WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | 1mm/min; ISO 527-2 |
Borealis GB366WG Polypropylene Compound, Glass Fiber Reinforced GB366WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ASTM D638 |
Plenco 7321 Phenolic, Granular, Transfer Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ASTM D638 |
Plenco 7476 Phenolic, Granular, Transfer Molded PLENCO 07476 is a cotton flock filled resole phenolic molding compound, with improved physical strength, crack resistance, and is resistant to soap and detergent solutions at elevated temperatures. .. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-25 HM PA6-GF25 Product description: Grilon BG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 25% glass fibers. Grilon BG-25 HM has the following important prop.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-35 PA6-GF35 Product description: Grilon BG-35 is a heat stabilized PA6 injection molding grade with 35% glass fibers. Grilon BG-35 has the following important properties: High stiffness Good surface finishEasy.. |
|||
Tensile Modulus | 6.90 GPa @Temperature 120 °C |
1000 ksi @Temperature 248 °F |
ISO 527-1/-2 |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 6.90 GPa @Temperature 120 °C |
1000 ksi @Temperature 248 °F |
ISO 527-1/-2 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK603 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 BK851 is a 20% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) 25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ISO 527 |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, DAM Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant.. |
|||
Tensile Modulus | 6.90 GPa @Treatment Temp. 70.0 °C, Time 864000 sec |
1000 ksi @Treatment Temp. 158 °F, Time 240 hour |
62% rel. humidity |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 31T1 MZ40 PA66, 40% mineral fiber, DRY Description: Flame retardant polyamide PA66, 40% mineral filled, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This.. |