Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers OPTRENE 10GF Polypropylene, 10% Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Ovation Polymers
Trade Name Optrene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers OPTRENE 10GF Polypropylene, 10% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties of chemically coupled glass reinforced (10 %) polypropylene with high strength and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 0.995 g/cc
0.995 g/cc
ASTM D792
Melt Index of Compound 13.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
50 mm/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
50 mm/min; ASTM D638
Tensile Modulus 1.70 GPa
247 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 55.0 MPa
7980 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.50 GPa
218 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 145 °C

@Thickness 3.20 mm
293 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved