Nylene® Vexel™ B12GF30 SA , 30% Glass Reinforced PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Nylene®
Trade Name Vexel™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Vexel™ B12GF30 SA , 30% Glass Reinforced PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vexel™ B12GF30 SA is a 30% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 227 °C
440 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
405 °F
ASTM D648