Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
NuSil CV-2946 Silicone, Thermally Conductive
General Purpose: Two Part Adhesive and Sealant Cure system: PlatinumInformation provided by NuSil
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Celanese Celanex® 3300-2FC PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300-2FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outs..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
RTP Company RTP 4607 FR Syndiotactic Polystyrene (SPS), Glass Fiber - Flame Retardant
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
RTP Company RTP 800 TFE 20 DEL Acetal (POM), Homopolymer - PTFE Lubricated - UL94 HB
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer  (Unverified Data**)
Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
RTP Company RTP 2105 TFE 5  Polyetherimide (PEI) Glass Fiber 30% - PTFE 5%  (discontinued **
Glass Fiber 30% - PTFE 5%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
RTP Company RTP 4300 B-360  Polysulfone/Polycarbonate Alloy (PSU/PC) Glass Fiber 30% - Flame Retardant
Glass Fiber 30% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information ..
Specific Gravity 1.53 g/cc

@Temperature 23.0 °C
1.53 g/cc

@Temperature 73.4 °F
ASTM D792
Kingfa PBT-G30 30% Glass Fiber Reinforced PBT
Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
MRC Polymers MAXNITEâ„¢ 550 GF30 PET, 30% Glass Mineral Reinforced
Information provided by MRC Polymers Inc.
Specific Gravity 1.53 g/cc
1.53 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1105-7860/GY7037 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
LG Chemical Lupox® GP-2151F General Purpose PBT, 15% Glass Fiber Reinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT
LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
SABIC Innovative Plastics Valox® 420M PBT (Asia Pacific)
30% GR PBTP. Easy flow/release. High stiffness and load bearing properties.This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
SABIC Innovative Plastics Valox® ENH4550 PBT
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
SABIC Innovative Plastics Valox® IQNH4550 PBT
Valox* iQNH4550 resin is a glass filled, non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% ..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
SABIC Innovative Plastics Valox® SHF436HR PBT
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
A. Schulman POLYBATCH™ White 8350/UV5 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8350/UV5 is a specialty white color concentrate containing an optimized blend of white and UV stabilizer based in polyethylene. POLYBATCH® 8350/UV5 has been designed to prov..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
A. Schulman POLYBATCH™ White 8350/UV5 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8350/UV5 is a specialty white color concentrate containing an optimized blend of white and UV stabilizer based in polyethylene. POLYBATCH® 8350/UV5 has been designed to prov..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
RTP Company RTP 1385 D TFE 10 Polyphenylene Sulfide (PPS), Carbon Fiber - PTFE Lubricated
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
RTP Company RTP 2202 HF TFE 15 Polyetheretherketone (PEEK), Glass Fiber - PTFE Lubricated
Specific Gravity 1.53 g/cc
1.53 g/cc
DIN 53479
Lubrizol ESTANE® 58564 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
RTP Company RTP 300 TC-C-20 Polycarbonate (PC), Thermally Conductive - Electrically Conductive
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
RTP Company RTP 1005 Polybutylene Terephthalate (PBT), Glass Fiber
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
RTP Company RTP 1385 TFE 15 SI 2 Polyphenylene Sulfide (PPS), Carbon Fiber - PTFE Lubricated - Silicone Lubricated
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
RTP Company RTP 2299 X 110551 Polyetheretherketone (PEEK), Carbon Fiber Reinforced - PTFE Lubricated
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
RTP Company RTP 205.3 TFE 15 Nylon 6/6 (PA), Glass Fiber - PTFE Lubricated