Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ASTM D638 |
Nylene® Vexel™ B12GF30 SA , 30% Glass Reinforced PBT Description: Vexel™ B12GF30 SA is a 30% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are.. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ISO value at 5mm/min. |
BASF Capron® GR40 HS 40% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR40 HS is a heat stabilized 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stabil.. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ASTM Data |
Dow Questra® QA802 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ASTM Data |
Dow Questra® WA205 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ASTM Data |
Dow Questra® WA550 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Strength, Ultimate | 121 - 207 MPa | 17500 - 30000 psi | Average value: 158 MPa Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | 5 mm/min |
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High.. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | |
AIM 80In/Pb15/Ag5 Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ASTM D638 |
Chem Polymer Durlex 730 G PBT, 30% Glass Fiber Reinforced A lubricated 30% glass reinforced PBT offering a balance of dimensional stability, tensile strength and high temperature performance.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 630 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 413 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ASTM D638 |
Chem Polymer Formax 630 G Acetal, 30% Glass Fiber Reinforced A copolymer acetal reinforced with 30% glass fiber for use in applications requiring great strength and rigidity.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ISO value at 5mm/min. |
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR40 is a 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is also ava.. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ NI-10CF/15T Nylon 6/10, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® NI-20GF/000 Nylon 6/10, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ASTM D638 |
PolyOne Lubri-Tech™ ES-20GF/08T Polyethersulfone - 20% Glass Fiber And PTFE
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 121 MPa | 17500 psi | ASTM D638 |
PolyOne Lubri-Tech™ ES-20GF/15T Polyethersulfone - 20% Glass Fiber Reinforced - 15% PTFE Lubricated
(disconti Data provided by PolyOne. |